Re: quickcast

From: RunWizard@aol.com
Date: Wed Aug 13 1997 - 16:22:12 EEST


I have not used the soligen process. I have seen the end result, and the
surface finish is pretty rough. May be acceptable for some applications, but
I would be unable to sell a casting to a aerospace company.