(no subject)

From: james mason (jim@foddesign.demon.co.uk)
Date: Fri Jun 26 1998 - 12:03:42 EEST


markschanze wrote:

> I would like to know if anyone has information on chemical removal of
> SLA
> epoxy from the inside of a metal coating. The SLA is used as a
> pattern and
> coated with thin metal. The idea is to produce tubes with very small
> I.D.
> geometries. Unless I am incorrect, I presume this is to small for
> Quickcast build style. The metal coating does not have a very high
> service
> temperature. If someone can help, I would appreciate some tips.
> Thanks.
> Mark Schanze
> Molding Technologies Manager
> CIVCO Medical Instruments
> marks@civcomedical.com
> 319 565 4447
>
> For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/

   Try contacting Jan Bettany martello.prototypes@dial.pipex.com
They do this all the time.
Regards James Mason @ FOD Ltd

http://www.fod.co.uk

For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/