Andy Scott wrote:
I understand that the mold will expand with temperature as well. So there
is
an optimum temperature that will yield the correct dimensions. Might take
you
a few test tries to find it though.
Andy Scott LMCO
Try this. Mix the same amount of urethane that would be used in the part.
Measure the exothermic peak. Cure the silicone mold at that temperature.
Heat the mold to this temperature when casting the urethane part.
Mark Schanze