0.100mm layers ?

From: Simon Slater (sslater@roushind.com)
Date: Thu Nov 12 1998 - 13:36:40 EET


Hello,

I am running an SLA-250/30 with SL5210 Ciba resin, can anyone help with the following:

Does anyone use regularly and successfully build SLA models using 0.100mm layers, if so what Z-wait, Pre-Dip, etc parameters do you use in part preparation ?

Has anyone been involved with temperature or humidity testing of SLA models using SL5210 resin ?

Ciba vs. DuPont. Does anyone have any preferences of Manufacturers of resins and what sort of results are you getting in comparative terms ?

Regards,
Simon D Slater
RP Development Engineer.