Hello to all,
1.
can anyone tell me the shortest time beetween layers for the differt RP
machines?
2.
What is the minimal layer-thickness for RP machines wich works well on
your machines?
3.
What is the cheapest stereolithographie epoxy-resin?
4.
Is there anyone of you who mixes the resin by himself?
5.
What wonderfull resin can i get when i accept a viscosity up to 20.000
mPas, and a time stability of 1 week
thanks to all for reading so many questions
and special thanks for all responser
Charly Fruth