Re: Titanium or Cobalt-chrome casting

From: Tom Richards (tomr@aicasting.com)
Date: Wed Feb 02 2000 - 19:17:41 EET


Ian: We can cast cobalt alloys #6, 23, & 25 in shell molds made from wax
impregnated SLS CastForm PS, Actua or Sanders patterns.

At 01:17 PM 2/2/00 +0800, you wrote:
>
>
>Dear rp-ml
>
>I am looking for anyone who has the ability to cast in titanium or cobalt
>chrome. I am doing some medical models for one of my colleagues in
>orthopaedic surgery. We have some small, detailed components that can be
>made in either SLS Trueform, SLA (the size of the components probably means
>that Quickcast is no benefit), or Sanders' wax.
>
>In the first instance I want to do a test run to check on process, costs,
>time, etc. This will lead on to a larger clinical trials batch.
>
>Can anyone help?
>
>IG
>
>Dr. Ian Gibson
>Associate Professor
>Department of Mechanical Engineering
>The University of Hong Kong
>tel: (852) 28597901
>fax: (852) 28585415
>mobile: (852) 98738281
>igibson@hkucc.hku.hk
>
>We work our jobs
>Collect our pay
>Believe we're ridin' down the highway when in fact we're slip-slidin away
>(Paul Simon)
>
>
>For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/
>
>

For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/



This archive was generated by hypermail 2.1.2 : Tue Jun 05 2001 - 23:02:44 EEST