Encapsulating metal parts in SLA

From: CES Sector DERA Malvern (spur8@dera.gov.uk)
Date: Wed Jan 24 2001 - 13:46:22 EET


Dear All

After seeing DERC's winning part (a complicated metal component successfully built into an SL part) in the Excellence Award at last years 3DSNASUG conference, I have been considering having a go myself as I can see potential benefits for my customer.

Has anyone tried this before? Success / Failure?
How is it done?
How difficult is it?
Could a Standard Licence user achieve this on a SLA250/50 with SL 5170 resin?

I would greatly appreciate any comments / help.

Unfortunately I've lost my delegates list from last year. Can someone help me find Paul Freeman in the UK? I believe that DERC have reformed and renamed themselves to PDR?

If possible could you please respond to imunwin@dera.gov.uk or contact me as below.

Regards

Ian Unwin IEng MIIE
Defence Evaluation & Research Agency
DSTL/Security Division
CES (ES) Dept. Room C811/12
St Andrews Road
Gt Malvern
Worcester WR14 3PS
United Kingdom
Tel +44(0)1684 896731
Fax +44(0)1684 896331
Email imunwin@dera.gov.uk
      or spur8@dera.gov.uk

-- 
The Information contained in this E-Mail and any subsequent correspondence
is private and is intended solely for the intended recipient(s).
For those other than the recipient any disclosure, copying, distribution, 
or any action taken or omitted to be taken in reliance on such information is
prohibited and may be unlawful.

For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/



This archive was generated by hypermail 2.1.2 : Fri Jan 04 2002 - 09:56:44 EET