Doug, post cured Nanoform has, in our very limited experience, and I'm
guessing 3D's Bluestone and Somos' other high temperature SLA resins
would probably work as well.
Ever onward! bob
________________________________
From: owner-rp-ml@rapid.lpt.fi [mailto:owner-rp-ml@rapid.lpt.fi] On
Behalf Of chathamres@aol.com
Sent: Friday, March 20, 2009 11:19 AM
To: rp-ml@rapid.lpt.fi
Subject: [rp-ml] Master Patterns for Spin Casting Molds
We have come across a Stratasys paper that states the use of their FDM
PC or PPSF materials are suitable for making master patterns for spin
casting, because these materials can handle temperatures up to 350
degrees F and pressures up to 3500 psi.
What other materials are available in the RP world that can compete with
PC or PPSF for making master patterns for spin casting?
Doug
________________________________
Live traffic, local info, maps, directions and more with the NEW
MapQuest Toolbar. Get it now
<http://www.mapquest.com/toolbar?ncid=emlwemqmq00000003> !
Received on Fri Mar 20 21:56:40 2009
This archive was generated by hypermail 2.1.8 : Thu Jan 07 2010 - 08:26:36 EET